FurnitureGuy
Industrial
Good morning...
We have received some Inconel 600 sheet for a job we are getting ready to fabricate. The material was purchased to ASTM B186. CMTRs (verified through PMI) show a Titanium content of up to 0.27% depending upon the sheet. Additionally, the Cobalt percentages are up to 0.52%.
Per the specification, there should, theoretically, be no Titanium or Cobalt in this material.
Does anyone know the effect these elements have on Inconel 600? Specifically: weldability, formability and any effect on the corrosion resistance.
Thanks in advance!!!
Cheers!
Mike
Michael Thompson
~~~~~~~~~~~~~~~~~~~
No honey, it's not the garage... it's my shop.
We have received some Inconel 600 sheet for a job we are getting ready to fabricate. The material was purchased to ASTM B186. CMTRs (verified through PMI) show a Titanium content of up to 0.27% depending upon the sheet. Additionally, the Cobalt percentages are up to 0.52%.
Per the specification, there should, theoretically, be no Titanium or Cobalt in this material.
Does anyone know the effect these elements have on Inconel 600? Specifically: weldability, formability and any effect on the corrosion resistance.
Thanks in advance!!!
Cheers!
Mike
Michael Thompson
~~~~~~~~~~~~~~~~~~~
No honey, it's not the garage... it's my shop.