AbolfazlYZP
Marine/Ocean
- Apr 4, 2020
- 7
Hi everyone
I have a model in abaqus standard, my model is a sandwich panel under in-plane compression and lateral pressure.
I’ve got this error:
Too many attempts made for this increment
and this warning:
Exhausted the contact constraint pool. Cutting back the time increment and redoing the current increment. Other wise, set the environment variable aba_gcont_pool_size to high or a numeric number (1,2,...) with 1 being equivalent to high.
The strain increment has exceeded fifty times the strain to cause first yield at 23 points
Excessive distortion at a total of 6319 integration points in solid (continuum) elements
My Model units is mm, the Young’s modulus and Yield stress in MPa.
also I have Cohesive layer and I used Quads Damage (Damage evolution and Damage stabilization Cohesive is also define for this) and Elastic with traction Type. for Enn and Ess, I did E/t cohesive layer for Enn and G/ t cohesive layer for Ess and Ett.
My step is General and Nlgeom is On. maximum number of increments is 300, initial increment size=0.01, minimum 1e-5.
In Interaction module I used Tie constraint for between cohesive and top layer and core layer. and coupling constraint is shown in below figure.
when I used coupling constraint and chose cohesive layer, my model errors for cohesive layer and I checked visualization module > Node sets > WarnNodeOverContieSlave. then I didn’t choose cohesive layer in coupling constraint. I figured out this error happened because the cohesive Layer was Slave.
my problem did not solve, but I didn’t get this warning again (WarnNodeOverContieSlave).
in Load module, My load is 0.01Mpa, and boundary condition shown in below figure. I define boundary condition with selected reference point for 3 side. for bottom side when I choose cohesive layer I’ve got warning incorrectDOF, so I did not select this layer.
I guess my problem is in coupling or boundary condition, but I don’t know what is it.
Can anyone help me?
I have a model in abaqus standard, my model is a sandwich panel under in-plane compression and lateral pressure.
I’ve got this error:
Too many attempts made for this increment
and this warning:
Exhausted the contact constraint pool. Cutting back the time increment and redoing the current increment. Other wise, set the environment variable aba_gcont_pool_size to high or a numeric number (1,2,...) with 1 being equivalent to high.
The strain increment has exceeded fifty times the strain to cause first yield at 23 points
Excessive distortion at a total of 6319 integration points in solid (continuum) elements
My Model units is mm, the Young’s modulus and Yield stress in MPa.
also I have Cohesive layer and I used Quads Damage (Damage evolution and Damage stabilization Cohesive is also define for this) and Elastic with traction Type. for Enn and Ess, I did E/t cohesive layer for Enn and G/ t cohesive layer for Ess and Ett.
My step is General and Nlgeom is On. maximum number of increments is 300, initial increment size=0.01, minimum 1e-5.
In Interaction module I used Tie constraint for between cohesive and top layer and core layer. and coupling constraint is shown in below figure.
when I used coupling constraint and chose cohesive layer, my model errors for cohesive layer and I checked visualization module > Node sets > WarnNodeOverContieSlave. then I didn’t choose cohesive layer in coupling constraint. I figured out this error happened because the cohesive Layer was Slave.
my problem did not solve, but I didn’t get this warning again (WarnNodeOverContieSlave).
in Load module, My load is 0.01Mpa, and boundary condition shown in below figure. I define boundary condition with selected reference point for 3 side. for bottom side when I choose cohesive layer I’ve got warning incorrectDOF, so I did not select this layer.
I guess my problem is in coupling or boundary condition, but I don’t know what is it.