We recently poured a 26' x 30' garage floor. The finishers were 1/2" low with their chaulk line in one spot. The last truck added to much water and should have been rejected but wasn't. I need to find a good topcoat product That will work from 1/2" to 1/16" coverage. I assume that for looks I will have to coat the whole floor. Any product recommendations or links would be greatly appreciated. The redimix company doesn't seem to have much info. I must be typing in the wrong search words, because I'm not getting results.
Thank you
 
try searching for either epoxy mortar or latex floor screed, this will be expensive and unfortunately highlights the need to get it right first time.

Zambo
 