2
We have a component that has failed and the report states that there has been a transcrystalline fatigue fracture of the component.
Any enlightenment on what mode of failure this is exactly would be greatly appreciated.
Thanks
 
Replies continue below

Recommended for you

This is the standard mode for metallic components subjected to cyclic loading.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
You can read more about this failure in the book.

"Mechanical Metallurgy" by Dieter.

Chocolates,men,coffee: are somethings liked better rich!!
(noticed in a coffee shop)
 
Thanks a lot. The references really helped.
 