In a Connection Substation, 3 generators of 100 MW each and 26 step-down transformers of 20 to 40 MVA are connected .
An usual test of measuring instrument over all the Station was performed.
One of the transformer connection [40 MVA Yo/D ] shows an odd result. One of the phases was less than 10% loaded.
The transformer its self does not show any damage or strange behavior. It seems that this transformer was over sized,
[future development was expected], so for years nobody paid attention.
Within few months the tap changer was checked so all the tank was open . On the medium voltage side[D] a phase
winding was founded interrupted[disconnected], may be from the beginning, as installed.
How could the transformer work properly for many years in this conditions?
An usual test of measuring instrument over all the Station was performed.
One of the transformer connection [40 MVA Yo/D ] shows an odd result. One of the phases was less than 10% loaded.
The transformer its self does not show any damage or strange behavior. It seems that this transformer was over sized,
[future development was expected], so for years nobody paid attention.
Within few months the tap changer was checked so all the tank was open . On the medium voltage side[D] a phase
winding was founded interrupted[disconnected], may be from the beginning, as installed.
How could the transformer work properly for many years in this conditions?