I am curious about people's experience using threaded rebar (14J and 18J) as anchors for transmission towers.
Do you specify the use of 14J and/or 18J threaded rebar for anchors? If so, have you had any push back from suppliers. My experience has been that these are getting harder and harder to source and can cost up to twice the amount of more typical F1554 heavy Hex Anchors (with the same diameter and length). Is anyone else having a similar experience, and if not where are you ordering your anchors from?
We recently had a vendor supply prices for both 14J anchors and 1-3/4" dia. F1554 Gr.55 Heavy Hex Anchors for a project with 27 anchor cages. The quote for 14J threaded rebar was $31,080.00. and the quote for 1 3/4" F1554 Gr 55 anchors was $18,700.00
Do you specify the use of 14J and/or 18J threaded rebar for anchors? If so, have you had any push back from suppliers. My experience has been that these are getting harder and harder to source and can cost up to twice the amount of more typical F1554 heavy Hex Anchors (with the same diameter and length). Is anyone else having a similar experience, and if not where are you ordering your anchors from?
We recently had a vendor supply prices for both 14J anchors and 1-3/4" dia. F1554 Gr.55 Heavy Hex Anchors for a project with 27 anchor cages. The quote for 14J threaded rebar was $31,080.00. and the quote for 1 3/4" F1554 Gr 55 anchors was $18,700.00