Could someone help me with the question below?
Is it acceptable, as alternative, carbon steel (A105 or WCB) hardfaced with stellite instead AISI 304 or AISI 316 in trim's valves?
I've faced a problem with a chinese manufacturer: I requested these trims types: AISI 410/STL, AISI 304 and AISI 316. Obs.: All shells are A216 WCB.
However they provided all trim's in A105 or WCB hardfaced + stellite. Have experienced something similiar to it? I would be very grateful for opinions.