Hello. I'm new here and I found this site greatly helpful to fresh engineers like me. Currently I'm testing few trusses made from relatively light and soft timber. Although they passed minimum requirement for strength, deflection etc given in Standards (BS and AS), they still generally failed at the member. Is it possible or practical in real situation to reduce the length of members by introducing more joints/splices to force the failure to the joints instead?
Expert opinions and any suggestions are deeply appreciated. Sorry for the language...