BillC
Materials
- Apr 18, 2001
- 8
1. How much U metal should be used to test out and verify that a new fire extinguishing agent is effective on U fires?
2. Should the U metal be machine cuttings? If yes how much should the cuttings weight? Should a solid piece of U metal be used?
3. If a solid piece of U metal is to be used in the fire extinguishing agent test what size should the metal be and how would it be ignited?
4. How many test should be required to qualify the agent?
2. Should the U metal be machine cuttings? If yes how much should the cuttings weight? Should a solid piece of U metal be used?
3. If a solid piece of U metal is to be used in the fire extinguishing agent test what size should the metal be and how would it be ignited?
4. How many test should be required to qualify the agent?