We are working on a Section VIII Div.1 carbon steel vessel that requires a Nickel alloy corrosion resistant weld metal overlay. For reasons I wont get into here we need to include the thickness of the overlay in the pressure design calculations as permitted by UCL-23(C). We would like to FCAW the overlay, but my AI has taken the following statement from UCL-23(c) to claim that the overlay MUST be deposited by a manual welding processes.
"The thickness of the corrosion resistant weld metal overlay cladding deposited by manual processes shall be verified by electrical or mechanical means."
To me this reads completely different. The shall in this statement does not seem to be referring to the welding process. The shall seems to be referring to the required verification based on "IF" the overlay is deposited manually.
Has anyone else run into this issue? Any code cases or interpretations that could help us argue that FCAW deposit of weld metal overlay is not prohibited by UCL-23(c)?
"The thickness of the corrosion resistant weld metal overlay cladding deposited by manual processes shall be verified by electrical or mechanical means."
To me this reads completely different. The shall in this statement does not seem to be referring to the welding process. The shall seems to be referring to the required verification based on "IF" the overlay is deposited manually.
Has anyone else run into this issue? Any code cases or interpretations that could help us argue that FCAW deposit of weld metal overlay is not prohibited by UCL-23(c)?