Hi, I have been asked to look into an issue in which I have little experience, since I primarily do building design. I will try to explain best I can.

At a wharf retrofit:
- 4' diameter by 16' long Foam Filled Fenders were added
- Behind each Fender, 1" thick UHMW panels were fastened to the existing Concrete Pier Wall (to protect it from the rubbing)
- Fenders are 'floating', anchored at each end to a chain, the chain fastened to embeds in the concrete wall
- I do not know any Ship Information
- I have cut sheets for the Foam Fenders, listing Engergy Absorption and Reaction Force

There is an issue with the UHMW Panel Fasteners:
- What size and spacing (and edge distance) is common?
- How do you determine the Design Forces (Longitudinal and Vertical) for the Fasteners? I have read through UFC 4-152 for 'Berthing Loads', but there are no specific formulas (just friction factors). Someone else told me to take the Foam Fender Reaction Force, multiplied by 20% multiplied by Friction Factor (0.20)......

Any help or insight is appreciated.
 
Replies continue below

Recommended for you

Hey, checking to see if anyone has insight on my questions above.

Thanks for any input.
 