Gents
We have to weld a 8x6" 12.7x11mm Reducer with a 6" Flange class 1500 thickness 18mm
The welding process is root GTAW then SMAW
On ASME B31.3 Par. 328.4.2 End Preparation (5): the preparation should be in accordance with ASME B16.25 Figure 5
I have some difficulty to deal with that and execute it on site
Need your advise
Thank you very much
We have to weld a 8x6" 12.7x11mm Reducer with a 6" Flange class 1500 thickness 18mm
The welding process is root GTAW then SMAW
On ASME B31.3 Par. 328.4.2 End Preparation (5): the preparation should be in accordance with ASME B16.25 Figure 5
I have some difficulty to deal with that and execute it on site
Need your advise
Thank you very much