What kind unit of measurement is used mainly for measuring the resistance to galling for metals?
 
Replies continue below

Recommended for you

pressure, like ksi or MPa.
But each test set up has its own base line.
You can't compare data from two different tests unless they were done using same machine and test setup.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 