We ordered API 5L Gr.B PSL-2 seamless pipes of varies sizes to a manufacturer.
As per project specification, pipes to be impacted at -18 deg C as per the requirements of API 5L.
Manufacturer done the impact test on the pipe of dia. greater than 3 inches pipes only and he refused to perform the impact test on 1" to 3" pipes.Manufacturer provided the table-22 reference of API 5L Clause -10.2.3.3.
Is it Acceptable?
We ordered API 5L Gr.B PSL-2 seamless pipes of varies sizes to a manufacturer.
As per project specification, pipes to be impacted at -18 deg C as per the requirements of API 5L.
Manufacturer done the impact test on the pipe of dia. greater than 3 inches pipes only and he refused to perform the impact test on 1" to 3" pipes.Manufacturer provided the table-22 reference of API 5L Clause -10.2.3.3.