1
- #1
adamgnt
Mechanical
- Sep 25, 2009
- 24
Hi all,
I am having some trouble with 316SS 10-24 FH screws backing out of their 316SS housing during system deployment. Looking to implement some sort of thread locking, but unsure of Loctite's performance in an open marine environment, and also if it arises any corrosion concerns (he housing are zinced). I know there are many types offered, I'm spending the morning looking through Loctite's site, all feedback of appropriate #'d product lines is welcome.
Thanks,
--Adam
I am having some trouble with 316SS 10-24 FH screws backing out of their 316SS housing during system deployment. Looking to implement some sort of thread locking, but unsure of Loctite's performance in an open marine environment, and also if it arises any corrosion concerns (he housing are zinced). I know there are many types offered, I'm spending the morning looking through Loctite's site, all feedback of appropriate #'d product lines is welcome.
Thanks,
--Adam