Transparent, lowcost UV resistant plastic?

<nbucska@pcperipherals.com>
 
Replies continue below

Recommended for you

PMMA, Acrylic, Methyl Methacrylate.

Regards
pat

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
ASA is also a good choice. Also materials that are average in UV can be modifed with the addition of additives to make them more UV resistant.
 
Not to forget PC...for extra strenghth and toughness. ASA is marketed on it's ability to retain colour. It has exceptional colour fastness properties and won't fade much over time even in direct sunlight.

Kieran
 
nbucska

My original answer was as brief as your question. If you want more info, please elaborate, particularly re application and environment of use.





Regards
pat

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 