Hello Everybody,

The coupling welded with Figure UW-16.2 F are subjected under any standard or any requirement about the dimension?
In particular related to the portion into the shell?


Thanking all for the cooperation,

Best Regards,
 
Replies continue below

Recommended for you

Hi,
Follow the requirements of UW-16(f)(3).

Notice the note in left bottom side of that Figure, you must use Standard Fittings: ASME/ANSI or Manufacturer's Standard.
 