It has been almost 5 years and I am still trying to get these small holes drilled in Tungsten ( see thread)
Basically ~5 - 10 micron hole in .300mm thick tungsten. Needs to be a straight thru-hole no taper and smooth edges. ( laser leaves a rough edge and a taper) I am using laser cut apertures but they are not perfect. Is there any new EDM technology? Has anyone aver rough cut 1st with laser then EDM to bore ?
Any help is very welcome
It has been almost 5 years and I am still trying to get these small holes drilled in Tungsten ( see thread)
Basically ~5 - 10 micron hole in .300mm thick tungsten. Needs to be a straight thru-hole no taper and smooth edges. ( laser leaves a rough edge and a taper) I am using laser cut apertures but they are not perfect. Is there any new EDM technology? Has anyone aver rough cut 1st with laser then EDM to bore ?