Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Viscosities of Water Treatment Chemicals

Status
Not open for further replies.

petriet1

Chemical
Oct 17, 2007
1
I'm working on some hydraulic calculations for 2% PAC in water, 50% Aluminum Sulfate (Alum) in water and 8% sodium hypochlorite in water. I'm trying to determine whether I should use the Darcy-Weisbach equation or if I can get away with the Hazen-Williams. I looked at the MSDS sheets and even the chemicals that are delivered as liquids do not have a reported viscosity. I've also contacted the manufacturer of the chemicals and haven't heard back. Can anyone tell me a good reference place to get the viscosities for these chemicals? Thanks everyone!!
 
Replies continue below

Recommended for you

The viscosity of 30% Aluminum Sulfate is:

1.41 cs/1.055 = 1.34 cP at 60 F (ref. Cameron Hydraulic Handbook, 4-37, 19th edition. For slurries, you can estimate the viscosity using the following:

Mori & Ototake

 