PAN
Mechanical
- Apr 25, 2001
- 549
For natural rubber lining or Poly Isoprene thickness of 3 mm, what is the recommended test voltage for holiday test? In my understanding the guide in NACE RP0274 is for pipe wrapping only. Testing with 14 kV might be too high voltage for this application. Is there another standard for specific application.