Hello!I work in Crude distillation unit.We have a small problem regardind the separation betwen water and hydrocarbons in reflux drum.The water is sent to sour water stripping unit with a high content of hydrocarbons.The reflux drum is a simple vessel as attached.We have a pH analyser that is coted with hydrocarbon and something that looks like soot.When is clean gives a reliable indication,but when coated the pH value rises.Do you have any suggestionfor a better separation?From where does this "soot" come?
Thanks for the help!
 
Replies continue below

Recommended for you

The soot sounds like Iron sulfide. The H2S is the system is combining with your steel to make it. I strongly suggest you UT your equipment.

 