weight of spray on fire proofing 1

Status
Not open for further replies.

Lutfi

Structural
Oct 20, 2002
1,035
I am away form my office and need the weight (psf) of spray on proffing.

Your help would be much appreciated.

Regards,
Lutfi
 
Replies continue below

Recommended for you

Lutfi - Per US Army COE USGF, for exposed structural components minimum applied dry density is 22 Lb/Cu Ft (Paragraph 2.1.1.2)

Minimum average thickness is 0.375 inches (Paragraph 3.4.4)

Works out to 0.69 Lb/Sq Ft (minimum)

Here is the link, in case you need more detailed info

[reading]
 
Slide Rule,

Many thanks! I was going to estimate about 3 psf and wait to verify.

Thanks again

Regards,
Lutfi
 
Lutfi....depends on whether cementitious or non-cementitious binder.

If cementitious (Grace Monokote or similar), should be between about 22 and 28 pcf. If non-cementitious(Cafco Blazeshield or similar), will be between about 12 and 15 pcf.
 