In the next few years, I'll be putting together my own weld shop, and was wondering about the possibility of building a gas manifold so I could selectively run argon, helium, CO2, oxygen, or nitrogen, or any mixture thereof. I'd probably use mass flow meters to control ratios. I imagine it the whole system could allow for fine tuning of gases for unusually delicate jobs. Can anyone think of any drawbacks or problems I'd encounter doing this? Or does somebody already offer such a system?