I needed help on understanding weld porosity.
What are the probable reasons for porosity to occur during MIG welding cold rolled sheets (2 mm thk).
Just to rule out the possibility of moisture, this problem creeps up even when the ambient temp during welding is as high as 35 deg C and the air is dry.