JT0202
Petroleum
- Mar 26, 2018
- 8
Looking to repair 4330mod 3/8" PJP on a 3" plate, V bevel.
YS 122ksi ; UTS 135ksi ; CVNs avg 50ftlbs @-4F ; 277/285 BHN
Will use E14018-G, although I have read also E8018-C3 can be used
preheat 600-650F
max interpass 750F
PWHT 1100F for 3hr
The results shall need to comply with CVNs avg 31 ftlbs @-4F ; 350 Hv
Any suggestions and/recommendations would be appreciated.
JT
YS 122ksi ; UTS 135ksi ; CVNs avg 50ftlbs @-4F ; 277/285 BHN
Will use E14018-G, although I have read also E8018-C3 can be used
preheat 600-650F
max interpass 750F
PWHT 1100F for 3hr
The results shall need to comply with CVNs avg 31 ftlbs @-4F ; 350 Hv
Any suggestions and/recommendations would be appreciated.
JT