Dear All,
I have a question about weld repairs on casting parts LCC. When we say weld repair means that if they find any defects then they have to grind out the defect and weld up the area. But the question is, during casting there are many small holes on the surface of part which most of casting suppliers weld up the area (many spot welding areas on part). Is it call weld repair too? My company doesnt accept any weld repair, so I need to know if this process of welding is common in casting.
Thanks.
Moe
I have a question about weld repairs on casting parts LCC. When we say weld repair means that if they find any defects then they have to grind out the defect and weld up the area. But the question is, during casting there are many small holes on the surface of part which most of casting suppliers weld up the area (many spot welding areas on part). Is it call weld repair too? My company doesnt accept any weld repair, so I need to know if this process of welding is common in casting.