Is Allowable to do a weld repair in defect type melt througth,using qualified FCAW process?
 
Replies continue below

Recommended for you

Most likely not. I would reject it.
Far better to cut it out.

OMG%20something%20else.png
 
Tks BigInch, we will consider your recomendation to stutus definition of pipes with this type of defective welds.
 