weldtek
Materials
- Feb 12, 2005
- 897
We have a customer requesting we attempt weld repair of some cracks in a slag crucible. It's cast iron ~ 3" thick. I had PMI done reporting the following, C > 3.50%, P .052, S .062, Mn .066, Si 1.5, Cu .23. I'm thinking we need to pass. Anybody have any thoughts?