we have received a pump casing casting from a foundry. it seems they did some weld repair on it.
The foundry did the hydro-test (1000PSI, 15mins) and it passed.
After we received the part and we redo the test after a few days.
It leaks around the weld repair.
What do you guys thinks. why it can hold the pressure in the 1st test? Is it because they did do proper PWHT after the repair?
Thanks
Past: Oil & Gas industry in Canada.
Present: Desalination pump manufacturer in the US
The foundry did the hydro-test (1000PSI, 15mins) and it passed.
After we received the part and we redo the test after a few days.
It leaks around the weld repair.
What do you guys thinks. why it can hold the pressure in the 1st test? Is it because they did do proper PWHT after the repair?
Thanks
Past: Oil & Gas industry in Canada.
Present: Desalination pump manufacturer in the US