I have to design a 32 tooth triplex 1.25 inch pitch with a plate insert instead of making it out of 1 piece because of cost purposes. To do so the insert will have to be fillet welded both sides of the plate, however, I have very little idea how thick the weld line should be and how much stress can it takes. The insert plate is 16 mm thick. Is there any formula that will help me calculate the radial weld and weld thickness?