We are trying to create a weld stud on .012" thick titanium, grade 3 or 4. We have a weld stud gun but contiuously keep blowing thru the metal. Also some of our weld studs are stainless steel. Does this pose a problem with different metals? Also is cleaniness an issue? Our engineering dept. had no problems with samples but we have had lots of troubles in the production environment. Thanks.
We are trying to create a weld stud on .012" thick titanium, grade 3 or 4. We have a weld stud gun but contiuously keep blowing thru the metal. Also some of our weld studs are stainless steel. Does this pose a problem with different metals? Also is cleaniness an issue? Our engineering dept. had no problems with samples but we have had lots of troubles in the production environment. Thanks.