I am aware of common practice whereby weld width is restricted to 3 times the diameter of the electrode used.
(ie vertical weave welding with a 4d electrode has a restriction on width to 12mm, anything wider has to be multi-capped!)
I am unable to find this restriction is ASME IX, the tank is also governed by API 620 code.

Please assist on this matter.
 
Replies continue below

Recommended for you

No such restrictions or limitations exist in Section IX. Any limit imposed would be put on the WPS at your discretion.
 