cjgrass

Industrial
Apr 8, 2013
34
Can a welder that has qualified on 8 5/8"OD x 0.500" pipe SVG 6G position using E8010-P1 for bead and hot pass and
E8018-C3 fill and cap be used to weld A572Gr50 1/2" plate SVG with backing using only E7018-1 in the 3G position?

Thanks

 
Replies continue below

Recommended for you

As the welder use F4 for his qualification (with backing of F3), yes he can weld using F4 with backing.

Regards,
AR
 