StoneCold
Chemical
- Mar 11, 2003
- 992
I walked into a project today where they were socket welding 2" pipe. They were tig welding the sockets which is a little odd in it's self but they were also welding the 304L pipe with ER 316L filler rod. I advised them that you would normally stick weld the sockets and that if you were going to tig the socket that the apropriate filler metal would be ER 308 or ER 309. Do you think there will be cracking at the root of the welds made with the 316L due to filler/base metal differences?
Thanks
StoneCold
Thanks
StoneCold