I have an application in which I have to resistance spot weld a 304 stainless steel screen grid to the inside of a D6ac cylindrical section that is about 0.055 inch thick and 5 feet long. The stainless screen is about 0.030 inch thick. The spot weld diameter will be about 0.090 inch. The D6ac will be heat treated to 220 ksi tensile strength. The welding will be performed after heat treating the D6ac.
Does anyone have an ideas as to whether it is possible to weld the 304 to the heat treated D6ac? Will there be a heat affected zone through the entire thickness of the D6ac or will the HAZ be confined to just below the weld?
Thanks for your help.
Paul
Does anyone have an ideas as to whether it is possible to weld the 304 to the heat treated D6ac? Will there be a heat affected zone through the entire thickness of the D6ac or will the HAZ be confined to just below the weld?
Thanks for your help.
Paul