conveyorbud
Mechanical
- Apr 23, 2004
- 21
We have a bull gear 214 tooth (142.667" pd) made of 4140 steel through hardened to 245-285 BHN. We are trying to weld it to a36 5/8" thick steel mixer drum. Both items must remain "very round". any suggestions?