Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations Ron247 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Welding carbon steel to manganese steel

Status
Not open for further replies.

georger

Mechanical
Sep 22, 2000
2
I am interested in the technology to join carbon steel (railroad rail) to manganese steel (a castings) using the flash butt weld process. Also any other welding process that can join these two steels reliably. [sig][/sig]
 
Replies continue below

Recommended for you

I work with Edison Welding Institute in Columbus, OH. We have done significant work with flash butt welding. I tried to forward your post to one of my collegues but something went wrong with the e-mail process.

If you would like some more information you should e-mail Tim Stotler. Tim_Stotler@ewi.org
He would be happy to answer any questions you may have regarding this application. [sig][/sig]
 