What are the rules and/or guidelines in API 650 of the shell plate of a storage tank having different grades of steel? Is there anywhere where it explicitly allows or does not allow this? We want to use a slightly higher grade on the lower courses and then a higher grade steel towards the top of the tank and cannot find any guidelines in the standard.

Thanks in advance
 
Replies continue below

Recommended for you

5.6.1.3 of API 650 specifically allows different shell courses to have different allowable stresses (i.e. different material grades).
 
It is very common to use higher strength material for the lower courses. If by grades you mean the API groups then it would be somewhat unusual to have a higher group number steel above a lower group number steel but there is no provision against it.
 
Thank you very much, I have now seen it.
 