Aloni
Mechanical
- Sep 7, 2013
- 36
Dear expert
I need to design a pressure vessel
Design pressure is 13.5 barg @ 350°c (195 psig@650°f)
My main concern is the body flange connection.
I have 2 option..
one :
is the to do an overlay with alloy 82 to the body flange 115 mm thk (about 5 mm thk overlay)
Second:
is to weld inconel 800 ring ,8 mm thk( kind of a stub end) with alloy 82 the body flange 115 mm thk.
The first option is more complicated due to the distortion on the 115 thk flange and due to the PWHT - that I won't to avoid.
The second option seems to be more practical but I am not sure if I need to perform PWHT also?
regarding the thermal expansion between the two materials, The weld in zone 1 will hold acc to the calculation ( the difference in expansion between the 2 material is 0.056 mm)
Please share your opinions
See the attach file.
Regards
aloni