Welding: LEAVE LOOSE condition at shipyards ??

Status
Not open for further replies.

researchguru

Structural
Nov 2, 2007
10
0
0
CA
I have some structural drawings for a ship. I'm wondering what it means when the drawings indicate LEAVE LOOSE for the stiffeners on the bulkheads.
 
Replies continue below

Recommended for you

If by flags, you mean "little triangles" (excuse my ignorance), then yes, there are flags.
:)

OK, so then that portion left "loose" will be welded at a later time during the assembly process. Pls correct me if I am wrong.

Thanks alot.

 
You need to look at the green AISC steel construction book, there is a weld symbol table in there that explains most things. The triangular 'flag' means that it is a site weld.
 