I have a situation here . Can anyone suggest that if we have to weld a SA-51670 plates with a SS316 backing strip then which electrode is best . Well I think root should be of 309 and then caping would be of 7018 OR complete 309 .. Can any one with welding knowledge suggest. I am also attaching a sketch of the weld detail.
Thank you and Best Regards
Assad
Thank you and Best Regards