Dear Material experts,

I have a pipe spool of SS321 being used for 1" riser along the flare stack.
I have short supply of material SS321, 1" pipe

Please suggest if I can use SS347 pipe spool available with me.
I need to weld the material as it has socket weld joints.

As per my study, E-347-16 welding rod is used for both, SS321 and SS347 material.

Please suggest if I can use SS347 pipe spool available with me.
 
Replies continue below

Recommended for you

Yes, indeed, the 347 pipe spool and weld rod will suffice in this application.
 
Should work fine. I see minimal risk.

= = = = = = = = = = = = = = = = = = = =