Dear Material experts,
I have a pipe spool of SS321 being used for 1" riser along the flare stack.
I have short supply of material SS321, 1" pipe
Please suggest if I can use SS347 pipe spool available with me.
I need to weld the material as it has socket weld joints.
As per my study, E-347-16 welding rod is used for both, SS321 and SS347 material.