Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations 3DDave on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

welding power supplies

Status
Not open for further replies.

bonzouk

Electrical
Apr 29, 2002
2
im doing a project on power supplies and need information about what voltage and current is used for various welding types .
ie 3v 200a = spot welding
i need info for all types including plasma , ultrasonic , spot ....
as you can see im not a welder !!!
 
Replies continue below

Recommended for you

There are two basic types of power supply used for welding: -

Constant current: where the current remains fairly constant and the voltage varies from typically 80v open circuit to 25V when welding. Usually the output from a transformer. It is used for manual welding process such as MMA(SMAW) or TIG(GTAW) etc.

Constant voltage: automatically maintains the arc gap. This is for automatic wire feeds such as MIG/MAG(GMAW) where changes in the wire feed alter the welding current, the welding current is set by the wire feed rate. As the arc gap closes the current reduces. As the arc gap increases the current increases.

A good book is the Lincoln 'welding procedure handbook'. It contains a good section on welding power sources. Its very cheap, and its available from