May 24, 2024 #1 duongwe Mechanical Jan 25, 2011 43 0 0 VN Dear Gents, WPS has been qualified ROOT/HOT/FILL/CAP = GTAW/GTAW/FCAW/FCAW. Now production the joint could be welded GTAW/FCAW/GTAW/FCAW or GTAW/GTAW/FCAW/GTAW? Thanks you.
Dear Gents, WPS has been qualified ROOT/HOT/FILL/CAP = GTAW/GTAW/FCAW/FCAW. Now production the joint could be welded GTAW/FCAW/GTAW/FCAW or GTAW/GTAW/FCAW/GTAW? Thanks you.
May 24, 2024 #2 david339933 Industrial Jun 15, 2011 1,204 0 0 CA As long as the process qualified with backing has backing, no problem. Upvote 0 Downvote
May 27, 2024 #3 MUHAMMAD FAHAD RANA Materials Dec 13, 2018 36 0 0 PK Agreed with David. I suggest, to rewrite WPS as per Actual process sequence for any query raised by client, As per code there is no issue. Fahad Upvote 0 Downvote
Agreed with David. I suggest, to rewrite WPS as per Actual process sequence for any query raised by client, As per code there is no issue. Fahad