May 20, 2024 #1 asotoe Materials Mar 25, 2009 3 0 0 CL Good day collegues and comunity, Please, anyone know the stainless steel ErCo2399?...i´m attaching some properties. We are searching the best electrode for repair a casting pieces. Thanks a lot in advance.
Good day collegues and comunity, Please, anyone know the stainless steel ErCo2399?...i´m attaching some properties. We are searching the best electrode for repair a casting pieces. Thanks a lot in advance.
May 20, 2024 #2 EdStainless Materials May 20, 2004 15,892 0 0 US As a cast alloy? What on earth is the microstructure? I have seen 30% Cr ferritic SS (<0.03% C) but never a martensitic. My first thought was an HD grade, but these usually top out at 0.50% C. How has your material been heat treated? Do you know? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed Upvote 0 Downvote
As a cast alloy? What on earth is the microstructure? I have seen 30% Cr ferritic SS (<0.03% C) but never a martensitic. My first thought was an HD grade, but these usually top out at 0.50% C. How has your material been heat treated? Do you know? = = = = = = = = = = = = = = = = = = = = P.E. Metallurgy, consulting work welcomed
May 20, 2024 Thread starter #3 asotoe Materials Mar 25, 2009 3 0 0 CL Good day,thanks for your reply. I didnt see the microstructure but for the hardness must be Q+T...by the way is a cast piece (pump body). Thanks. Upvote 0 Downvote
Good day,thanks for your reply. I didnt see the microstructure but for the hardness must be Q+T...by the way is a cast piece (pump body). Thanks.