Welding Symbols

Ramadan Ahmed

Mechanical
May 16, 2024
15
SA
Good evening all,

I'm working on a design which is a 2.5mm Aluminum that is bent in various location to form a box. i want to use welding symbols (I'm new to welding symbols) in Sledworks, but I'm not sure which symbol to use in these areas shown. can someone help me with this please

Thank You

weld 2 .pngweld 1 .png
 
Replies continue below

Recommended for you

By inspection I think those tight bends will cause cracking depending on the material and the orientation .
Transverse direction is more vulnerable to cracking in rolled plate.

The loading in service will determine if fatigue failure is a consideration, and that can have profound effects on the weld design and weld process required.

AWS A2.4 shows most of the possible weld configurations and the symbols that define them.

Some more technical details would help others provide useful answers.
I wonder if you have the details you need.
 