Hi there, I am trying to approximate a wet concrete load behind a wall during a pour.
Would I just consider the wet concrete load as 25 kN/m3 and calculate as a normal earth pressure or would I need to consider 24 kN/m3 + 10 kN/m3 (where the 10 kN/m3 is the density of water and 24 kN/m3 the density of concrete).
Thanks
Would I just consider the wet concrete load as 25 kN/m3 and calculate as a normal earth pressure or would I need to consider 24 kN/m3 + 10 kN/m3 (where the 10 kN/m3 is the density of water and 24 kN/m3 the density of concrete).