We would like to all expertise explore the defect of welded after the pressure test is attached.
All in your advice will be information and preventive to our team

Thank you very much.
1754_ytxnhj.jpg

6767_waw8ax.jpg

6766_txvpom.jpg
 
A young engineer dropped into this, should look for other employment. This is more than a bad welder, it's a systemic QA/QC failure, from the top down.
 
He misspelled ‘defecation’ in the OP title, but that is certainly what those welds look like.

 
MJ,

Agree, in these situations it's usually the boss who should be blamed.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Amen, IRONIC, Amen !!!!

MJCronin
Sr. Process Engineer
 
This material should go to scrap in its entirety, including the manufacturer.

Regards
 
Where do we start....
Porosity
Lack of fusion
Lack of penetration
Profile

All bad.

 
Ron said:
Where do we start....
Porosity
Lack of fusion
Lack of penetration
Profile

Career choice...