Hi experts,
I found the "Guaranty" in the datasheet of LB-52NS (E7016-G) SMAW welding electrode. So what does it mean?
In ASME II part C, SFA5.5, Table 2, I see that the weight percent of Si is 0.8min. But I see that in most of certificate of E7016-G, the weight percent of Si is 0.3x.
Please help me more understanding it.
Thanks experts.
LB-52NS_a_tddke6.png

LB-52NS_b_olxqrz.png
 
Replies continue below

Recommended for you

They're just stating what their self-imposed limits are for that particular product. It does not necessarily have to align with the table, the manufacturer is being more stringent with their chemistry than what A5.5 allows.
 
@CWEng : thanks. Now I get that footnote already.
@Mr168 : thanks for your help.
 